Nimonic 80A

Features:

Alloy 80A (Nimonic® alloy 80A) is a wrought, age-hardenable nickel-chromium alloy. Alloy 80A is similar to alloy 75 but made precipitation hardenable by additions of aluminium and titanium. Alloy 80A has good corrosion and oxidation resistance and high tensile and creep-rupture properties at temperatures to 815ºC (1500ºF). Vacuum refined versions are also available. Alloy 80A is used for gas-turbine components (blades, rings, discs), bolts, tube supports in nuclear generators, exhaust valves in internal combustion engines and has many other offshore/marine, automotive and electrical applications.

 

Nominal composition,%

Alloy 

designation

C

Ni

Cr

Co

Pb

Fe

Al

B

Ti

S

Mn

Cu

Zr

Si

Alloy 80A

Nimonic 80A

0.1

Bal

18~21

2

0.002max

3max

1~1.8

0.008

1.8~2.7

0.015

1max

0.2

0.15

1

 

 

Typical Mechanical Properties:

Material

Condition

Ultimate Tensile Strength ksi

Yield Strength ksi

Elongation on 4D (min)

Hardness min

Nimonic 80A

Alloy 80A

Solution Annealed & Precipatation Treated (aged)

145

90

20

300 HV

 

Availability:

Alloy 80A is available in Round Bar, Flat Bar, Rod, Tube, Plate, Sheet, Strip, Forging Stock and Wire.

 